方道城(1993—)男,副主任,助理工程师,332600江西省九江市。江西某钨钼矿综合回收钨钼浮选工艺研究方道城(江西都昌金鼎钨钼矿业有限公司)摘要为合理利用江西都昌金鼎钨钼矿业某钨矿矿石,采用浮选工艺对该钨矿中的钨、钼回收开展了可选性试验。试验结果表明:以2#油为起泡剂、柴油为捕收剂,在磨矿细度-0.074mm60%的条件下,采用1粗2扫、钼粗精矿浓缩粗选后4精2精扫浮选流程,可获得钼品位43.13%、钼回收率50.65%的钼精矿;以纯碱+片碱为调整剂、脂肪酸+植物油酸为捕收剂,采用选钼尾矿1粗2扫、钨粗精矿加温粗选后4精2精扫浮选流程,可获得钨品位60.08%、钨回收率81.28%的钨精矿,获得了良好的试验指标。关键词白钨矿辉钼矿钨钼分离浮选工艺DOI:10.3969/j.issn.1674-6082.2023.09.037FlotationProcessTestofComprehensiveRecoveryofTungstenandMolybdenumfromaTungsten-molybdenumMineinJiangxiFANGDaocheng(JiangxiDuchangJindingTungstenMolybdenumMiningCo.,Ltd.)AbstractInordertomakerationaluseofatungstenorefromJiangxiDuchangJindingTungstenMo⁃lybdenumMiningCo.,Ltd.,awashabilitytestwascarriedoutontherecoveryoftungstenandmolybdenumfromthetungstenorebyflotationprocess.Undertheconditionsof2#oilasfoamingagent,dieseloilascol⁃lectorandgrindingfinenessof-0.074mm60%,theflotationprocessofoneroughingtwoscavengingandfourcleaningtwocleaningscavengingaftermolybdenumroughconcentrateconcentrationandroughingwasadopted.Molybdenumconcentratewithmolybdenumgradeof43.13%andmolybdenumrecoveryrateof50.65%couldbeobtained.Usingsodaash+flakealkaliasregulatorandfattyacid+vegetableoleicacidascollector,theflotationprocessofoneroughingtwoscavengingformolybdenumtailingsandfourcleaningtwocleaningscavengingaftertungstenroughconcentrateheatingroughingwasadopted.Tungstenconcentratewithtungstengradeof60.08%andtungstenrecoveryrateof81.28%wasobtained.Thetestindexisgood.Keywordsscheelite,molybdenite,tungstenandmolybdenumseparation,flotationprocess总第653期2023年9月第9期现代矿业MODERNMININGSerialNo.653September.2023我国是钨资源大国,钨资源储量世界第一。然而,随着社会和经济的高速发展,我国钨资源消耗量逐渐增多,占世界的40%,易开发利用的黑钨矿已接近枯竭,...